For a steel alloy it has been determined that a carburizing heat treatment of 10.8 h duration will raise the carbon concentration to 0.310 wt% at a point 1.30 mm from the surface. Estimate the time necessary to achieve the same concentration at a 4.80 mm position for an identical steel and at the same carburizing temperature.

Respuesta :

Answer:

135 hours.

Explanation:

See attached picture.